Dear Zhu, Alumina coated tungsten boats lasts longer than simple tungsten boats for Ni evaporation. They are available from Kurt J. Lesker. Oray Orkun Cellek > Re: I am using E-beam to evaporate Ni. The crucible is > Re:made of tungsten. But it seemed that fused Ni could > Re:"eat" tungsten. I wonder whether they have formed some > Re:kind of alloys. Should I replace the tungsten crucible > Re:by other metals, such as molybdenum? Thank you very > Re:much.