durusmail: mems-talk: ebeam Ni, crucible?
ebeam Ni, crucible?
2005-05-28
ebeam Ni,crucible?
2005-05-29
2005-05-29
2005-05-28
2005-05-31
ebeam Ni, crucible?
Shay Kaplan
2005-05-29
You should use vitreous carbon crucible
shay

-----Original Message-----
From:  X.P. Zhu
Subject: [mems-talk] ebeam Ni, crucible?

Dear members,
   I am using E-beam to evaporate Ni. The crucible is made of tungsten. But
it seemed that fused Ni could "eat" tungsten. I wonder whether they have
formed some kind of alloys. Should I replace the tungsten crucible by other
metals, such as molybdenum? Thank you very much.
reply