PDMS bonding to glass
2005-06-01
antireflection coating?
2005-06-03
2005-06-07
PDMS bonding to glass
mbeggans@biovalve.net
2005-06-01
UV/Ozone clean for ~ 1min or so and immediately contact the PDMS and
glass. It's not a permanent bond (you can peel the PDMS off afterwards).
It will hold up to high pressures (as in a microfluid channel), but not
high shear stresses.

Mike