Hi, I have started working on thin film sol-gel PZT. I searched either in the web and our list but cannot find satisfactory information in detail. I need to etch PZT on Si/SiO2/Ti/Pt wafer using dry or wet etch methods. But our RIE has only SF6, CHF3, and O2. So I am looking for a wet etch solution. I tried different solutions such as 10:1 BOE, 2:1 HCl:DI, and 50:50:1 DI:HCl:HF but could not get fine results. Because etchant should be selective to Pt, I am trying to avoid HF contents. If anyone has some idea or some experience to share, I will be appreciated. Thanks, Tolga