Hi Mohammed, You could always place down oxide or place the wafer in a prime oven to increases hydrophillicity . Phillipe Tabada >From: "mohammed ashraf">Reply-To: General MEMS discussion >To: mems-talk@memsnet.org >Subject: [mems-talk] microlens >Date: Mon, 27 Jun 2005 11:07:04 +0000 > >Hi all >I need to decrease the contact angle while reflowing microlenses.Can >somebody suggest a practical way of increasing the hydrophillicity of >Si-substrate wrt PR(AZ9260cp). >Regards >Mohammed Ashraf > >_________________________________________________________________ >44 Million Items on Sale.What Are you Looking for? >http://adfarm.mediaplex.com/ad/ck/4686-26272-10936-377?ck=44MilItems Find >it on eBay.in! > >_______________________________________________ >Hosted by the MEMS and Nanotechnology Exchange, the country's leading >provider of MEMS and Nanotechnology design and fabrication services. >Visit us at http://www.mems-exchange.org > >Want to advertise to this community? See http://www.memsnet.org > >To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk