durusmail: mems-talk: nanoparticle spin coating
Your thoughts on this pls
nanoparticle spin coating
2005-06-30
2005-07-04
nanoparticle spin coating
Erik Jung
2005-07-04
Spin coating might not be the best choice. A well established method for
single layer deposition is e.g. the LagnmuirBlodget method. Also Self
Assembled Monolayer technique (modifying your nanoparticle receiving layer)
will perhaps help.
Regards!
Erik


-----Urspr|ngliche Nachricht-----
Von: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org]Im Auftrag von li cai
Gesendet: Donnerstag, 30. Juni 2005 05:13
An: mems-talk@memsnet.org
Betreff: [mems-talk] nanoparticle spin coating

Does anyone know how to spin coat an uniform single layer nanoparticles?

Thanks,

Li
reply