PDMS to PDMS bonding
2005-07-07
2005-07-11
Resonant Frequency Measurement
2005-07-13
PDMS to PDMS bonding
Edward Castellana
2005-07-07
Vishwa,

You are plasma treating too long.  Try only 15 seconds.  I
also sugest skiping the ethanol cleaning.  Just rinse the
PDMS with purified water and dry it with N2 gas.

Ed

  >Hi,
  >I have been having problems with bonding PDMS to PDMS.