Lee Pang
2005-07-07
I agree with Ed.  15-30 secs of plasma is sufficient.  I've also found
that allowing the bond to "cure" for 10-30mins after being brought in to
contact helps, especially if the bonding surface has a relatively large
area (~2-3cm^2).

Lee