Hi everyone, we are trying to replace SJR 5740 with SPR 220-3 for electroplating process. However we observed that SPR220 can not withstand inside the cyanide gold plating solution even for a hardbake temperature of 120 C for 12 hours. For SJR 5740, we managed to achieve very stable features for a plating duration of 30 minutes. The hardbake temperature for SJR 5740 is 80 C for 12 hours. Do you have any experience about the durability of SPR 220-3? Do you have any alternatives to be used as mold photoresist for 30-40 minutes of gold plating? Thanks in advance. Mehmet Unlu Research Assistant Ph. D. candidate MEMS-VLSI Group Electrical-Electronics Eng. Dept. Middle East Technical University Ankara, Turkey