Has the resist been opened for longer than a year? If yes, I would say it is probably due to excess water absorbed from the air in the resist. You are trying to push the resist to the limits (thick layer, it's designed for 1.1um thickness, btw), image reversal is always tricky. What are your feature size? If you notice ragged walls, I bet it's small. And with a 2 year too old resist - no wonder it's not working very well. The dehydration bake prior to application of PR is mighty critical. -----Original Message----- From: Krishna Vummidi Subject: [mems-talk] 5214E resist Im using 5214E in image reversal mode. below is my process On Si wafers (BOE, Acetone, IPA clean) spin: 2000rpm (2 um) soft bake: 110C for 1m30s expose for 10.4 sec at 8.7 mW/cm2 (i-line) Reverse bake: 118-120C for 1m flood expose: 90 sec same lamp power as above dev: MIF-327 or AZ 400K (1:4) for 1m After i develop, my resist doesnt seem to have a straight edge. the walls are really rugged. the expiration date on the resist is 2003 march. is that an issue or do i have to correct my process. or is it the surface preparation of my wafer. is the dehydration bake of Si wafer before process that critical. The resist development seems to be better in case of normal positive exposure. any thoughts, ideas are much appreciated. thanks, krishna