Are you sure it isn't POPOTASSIUM IODIDEE:) -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Dean Hopkins Sent: Monday, July 25, 2005 10:09 AM To: mems-talk@memsnet.org Subject: [mems-talk] Re: Gold etching (Nik Dee)/ David Nemeth "Theres is an Iodidee/Ammoniumum Idodide etch" Ummm NO!!!! Ammonium Iodide is a very sensitive explosive!!!! Should be: Iodine/POPOTASSIUM Iodide etch.