I am looking for a low refractive index epoxy and or glue for some of my optical device applications. This material is required to have a good heat resistance upto 250C and a good processability for spin coating, bonding etc. Can some one help! Would be happy to receive a response from material suppliers. Best Regards. GV. Please respond to gvis03@yahoo.com if possible.