Sarkar, Also bear in mind that SU-8 has a thermal cross-link reaction as well (at 120C, if I remember correctly, although it may be as high as 150C). It may have been that the temperature the SU-8 saw was too high. Best Regards, Chad Brubaker -----Original Message----- From: Jobert van Eisden Subject: RE: [mems-talk] Metal deposition on unexposed SU-8 Hi Aniruddh, I have done this using an e-beam evaporator. Depending on accelerating voltage there will be some radiation, but in my case not enough to expose the SU8. The problem I found with this is that during the post exposure bake the SU8 will shrink, buckling your film on top. Jobert van Eisden SUNY Albany