A negative sloped side wall is essential Using image reversal the flood exposure controls the side wall angle from a +22 degrees through vertical to -22 degrees or slope back. Using this for example Cray Research when they produced chips for the Cray super computer had a number of image reversal systems and were producing 0.1 Micron metal lines. Other customers use the vertical side walls for plate up and produce 30 Micron thick copper with vertical walls inside 40 micron vertical wall trenches. Bill Moffat, CEO Yield Engineering Systems, Inc. 2185 Oakland Rd., San Jose, CA 95131 (408) 954-8353