I searched the internet and found a Silicon-Aluminum phase diagram. Here is the URL: http://www2.umist.ac.uk/material/research/intmic/phase/alsidiag.htm The eutectic composition is approximately 87 wt% Al and the eutectic temperature is 660C. -Scott -----Original Message----- From: Gary Sent: Friday, August 12, 2005 10:46 AM To: 'General MEMS discussion' Subject: RE: [mems-talk] eutectic point of silicon-aluminum Li, These materials don't truly alloy, hence there is no eutectic, The "alloys" are really finely divided mixtures, and manufactured using an atomization process.