There is a possibility to oxidize silicon in hot nitric acid (115°C). After 10 minutes we measured a SiO2 thickness of about 30 nm. I don't know what will happen to gold but theoretically it should not be affected. Best mic -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of cyyfq@bu.edu Sent: Freitag, 9. September 2005 18:13 To: General MEMS discussion; Laetitia Philippe Cc: mems-talk@memsnet.org Subject: Re: Rép. : [mems-talk] Oxidize Silicon I have Gold pattern on the sample and meling point of Gold is 1064oC. if I want to do it at 1000oC or 900oC, what should be the time by your expection? I do not need to be accurate. 20-50nm of SiO2 is fine