I am a PhD student working on a new electroless etch stop technique.
Could you help me with the following problem:
What kind of metal process do I need to get a gold layer on silicon
which survives KOH or TMAH at high temperatures. We have tried
evaporated Au/Cr but that comes of after a few hours?
If you can help me please e-mail:
0000,0000,C0C0c.m.a.ashruf@et.tudelft.nl
Thanks
Try out Ti/W as a first layer. It works for Pt electrodes in KOH....