I was one of the person who asked this question. From what I was told you
can't crosslink PMMA by using UV. If you find something on the contrary
please let me know
Thanks

 Fabio

--
Fabio Altomare
Post Doctoral Research Associate
Physics Department
Duke University



On Thu, 1 Dec 2005 cyyfq@bu.edu wrote:

> Hello all:
>
> I want to crosslink PMMA and I know high dose e-beam exposure can do
> this.
> but what I want is to cross link large area of PMMA which can not be
> done by e-beam.
>
> can UV work? somebody asked this before but I could not find the
> answer.
>
> what should be the condition?
>
> any suggestions are welcome.
>
> best
>
> Yu Chen
>