Hi, Bill,
Thank you for your reply. It seems that my responce didn't get through
MEMS talk few days ago.
I think I didn't describe my question well at the beginning.
On top of gold, there is an electroplated and patterned copper layer.
I want to remove the exposed gold, but not the copper.
I doubt that I can use lift-off technology though.
That is why I want to see if I can use Argon plasma. My copper layer is
much thicker than gold.
Any suggestion?
Richard
----- Original Message -----
From: "Bill Moffat"
To: "General MEMS discussion"
Sent: Wednesday, December 07, 2005 8:56 AM
Subject: RE: [mems-talk] Argon plasma for gold etching
> Richard,
> Argon is inert, Argon plasma is electrically active but still
> inert. It can sputter but the amount removed is small. Think maybe an
> Angstrom a minute in a low energy hybrid plasma descummer, maybe 10
> Angstroms a minute in a high intensity single wafer resist stripper.
> With an over $1M Applied Materials 5000 R.I.E. think maybe 100 Angstroms
> per minute. All of which is cost and time prohibitive. Think metal lift
> off for definition better than 0.08 micron thicknesses up to 20 to 30
> Microns of copper. 10 Microns of Tantalum for flip chip bumps or well
> over 5 microns of Gold. Contact me for more details.
>
> Bill Moffat, CEO
> Yield Engineering Systems, Inc.
> 2185 Oakland Rd., San Jose, CA 95131
> (408) 954-8353
>
> -----Original Message-----
> From: mems-talk-bounces@memsnet.org
> [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Richard Chang
> Sent: Tuesday, December 06, 2005 4:07 PM
> To: General MEMS discussion
> Subject: [mems-talk] Argon plasma for gold etching
>
> Hi, All,
>
> I want to use argon plasma to etch away exposed gold.
> My thickness of gold is 1 micron.
> Does anybody have the recipe for the plasma etching, like RF power,
> pressure of Argon?
> How long it might take to etch away 1 micron thick gold?
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community? See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>