PRAMOD GUPTA
2005-12-13
We are looking for a masking material or resin to mask certain area of the metal
or/and SS tube before it goes to Ni or Gold Electroplating bath. Could you
please suggest some materials or technique or any electroplating shop who can do
both masking and electroplating for us?

Shile  wrote:
    I don't recall mentioning an SU-8 remover.

-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org] On Behalf Of P.E.M. Kuijpers
Sent: Sunday, December 11, 2005 10:20 PM
To: General MEMS discussion
Subject: Re: [mems-talk] SU-8 remover

Hello,

What is the SU-8 remover you mentioned!
Is this for removing fully cured SU-8?

Thanks in advance.
Peter Kuijpers