Bond strength can be measured by a tensile tester. Mount test samples and pull from two opposite directions. A good reference Book is Semiconductor Wafer Bonding by Tong and Gosele. Best Regards, Chad Brubaker -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Vikram Patil Sent: Monday, December 19, 2005 8:10 PM To: mems-talk@memsnet.org Subject: [mems-talk] wafer level bonding Hi all! I am trying to gather some references for wafer level adhesive bonding. Can anyone tell me how much bonding strength is good? Or How does anyone determine good bond stength value?