durusmail: mems-talk: Removing dry resist
Removing dry resist
2005-12-21
2005-12-21
2005-12-21
2005-12-22
2005-12-23
2005-12-23
Removing of Polycarbonate (PC)
2005-12-25
2005-12-22
Removing dry resist
Sven Holmström
2005-12-22
Thanks for the answers. Most of you say Oxygen plasma, which we have
been thinking of too. But as of now we don't have that available
locally (we could send it away though, for certain cost).

On 12/22/05, Shile  wrote:
> Try a photoresist stripper.  I'm not aware of acetone as an ingredient
> in any commercially made resist stripper.

Does anytone else have an opinion about this. Might it be possuble to
use a stripper when the resist is totally dried out? (BTW, we know
that acetone works when the S1813 is not too aged.)

/Sven
reply