Chao, Electroless plating on SU-8 is pretty tricky becasue the surface is exteremely smooth. You can roughen the surface using oxyen/Fluorine plasma or some wet process like permanganate etching. Look for papers from Georgia Tech (I am sure there are others too) for more specific details on roughening process. Regards, Dev