I have bought down to 0.2mm 4x4" sheets Schott borosilicate from S.I.
Howard Glass. They are pretty painless to work with, but maybe not if
you are outside the US. Shipping without breakage can be a challenge.

http://www.howardglass.com/D263.html

Linas.

-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org] On Behalf Of gillot
Sent: Saturday, December 31, 2005 10:14 PM
To: General MEMS discussion
Subject: [mems-talk] .3/.5 mm thick glass


Dear List,

Happy new year !

I am looking for plate glass with a thickness of .3 or .5 mm to be
sputtered, but it seems that it doesn't exist on earth...