Hello,

I am trying to fabricate a suspended aluminum (99% Al, 0.5% Si, 0.5% Cu)
structure, 1.15um thick on a silicon wafer.  The suspended length is
approximately 130um.  After the structure is released etched from the
silicon using XeF2, the aluminum bridge bows and twists due to stresses.
What causes this and how can I prevent it?  Thank you.

Sincerely,

Robert Dean