Gabe/Silvan,
            Try image reversal for dimensions down to 800 Angstrom lines
and spaces and resist thicknesses of up to 40 microns. Contact me for
more details. bmoffat@yieldengineering.com


Bill Moffat, CEO
Yield Engineering Systems, Inc.
2185 Oakland Rd., San Jose, CA  95131
(408) 954-8353