> I am looking for wet etching techniques for etching Si(111) wafers. > can anyone provide me leads for the same. we use hf:nitric:acitic at a low temperature. works good. Generally chromium is better..or Titanium., Then You can deposit the metal you want by metallization.. Regards., Balasubramanian Mcmaster university.