Hi everybody I'm going to do some process with SiC wafers. The problem is the machine I can use are designed for 4 inch wafers .. and my SiC wafers are 1.3 inch cutted in four !!! For the sputter deposition machine, no problem, I can use a metal wafer with clips to fix the little wafer. For the implanter, I can't use that and I must stick the wafer on a 4 inch Si wafer. The only way I see is to use resist. Do you have other ideas ? Did somebody use resist as paste ? How did you that ? Many thanks per advance, Christophe Sudre -- _______________________________________________________________________________ | Dr Christophe Sudre Fax : 353 21 270271 | | Research Scientist Phone : 353 21 904079 | | University College Cork WWW : http://www.nmrc.ucc.ie/| | National Microelectronics Research Center Email: csudre@nmrc.ucc.ie | | Lee Maltings, Prospect Row | | Cork, Ireland | |_______________________________________________________________________________ |