Hi Do you have any idea whether Balco (Ni 70% + Fe 30%) wire of 0.002" dia can be bonded on Ni/Au pads by using thermosonic/ultrasonic technique or not? If yes, who can do it? With regards, David Nemethwrote: One possible solution would be to use a very small dab of silver conductive epoxy after bonding. Epotek makes such an epoxy, although it is also available from a variety of other sources. David Nemeth Senior Engineer Sophia Wireless, Inc. 14225-C Sullyfield Circle Chantilly, VA 20151 -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org]On Behalf Of Stanley R. Shanfield Sent: Monday, February 27, 2006 2:50 PM To: mems-talk@memsnet.org; mems-talk-owner@memsnet.org Subject: [mems-talk] Wire bonding problems We are trying to manually wire bond to thin (~.2 micron) Pt/Au on glass. Although we get good bonds on test wafers at the time the metal is deposited, the bonding is very unreliable after it has gone through more processing (i.e. at wire pull test, the wire falls off, leaving the pad intact,& undamaged; or the pull strength is low). The wafer sees anodic bonding conditions at one point in our process sequence, and the sawing process can leave scratches on the pads (the scratches do not penetrate the metal). Going up in bonding energy, time and force is a concern, since the glass sometimes forms fissures under the bonding area at more extreme bonding conditions, and a subsequent wire pull creates a pull-out from the glass. It does not seem to help anyway. These bonds have to survive a ~350C temperature excursion, so a pull-out is a concern. Has anyone ever dealt with a problem like this? Any advice or observations? You input would be much appreciated!