Hi, all,
   I need some help in thermal growth SiO2, including the detailed steps
(for example, if the Si sbustrate are directly interted into and removed
out from the tube furnance or not), the rough growth rate.

   I want to use water steam to promote the oxidation.

Thanks for helps.