>I am attempting to spin AZP4620 at ~10um. I have used many variations >on the manufacturer's specified recipe for a 10um coat. After the >prebake the uniformity is not that good. I would like uniformity as I >would expect in OCG 825 or Shipley 1818. Q1: what Should I expect for >uniformity. Q2: are there any key points in the application of the PR >that you can share. THANKS > The trick is the baking. You may need long bake time and possibly lower bake temp. chia-lun ___________________________________________________________________ Chia-Lun Tsai, PhD School of Electrical Engineering 402 Phillips Hall Phone: (607) 255-0102 Cornell University Ithaca, NY 14853-5401 ct61@cornell.edu