Hi Paul

If I remember correctly it is approximately 0.1 um /min depending on how
fresh the solution is.

Paul Monaghan wrote:

>Gareth,
>
>out of interest, what sort of etch rates do you get for sodalime glass with
>that etchant?
>
>thanks,
>
>Paul
>