durusmail: mems-talk: Can PMMA work as mask for dry etching on II-VI(ZnSe based) semiconductors?
Can PMMA work as mask for dry etching on II-VI(ZnSe based) semiconductors?
2006-05-17
Can PMMA work as mask for dry etching on II-VI(ZnSe based) semiconductors?
jiaxing Yang
2006-05-17
I tried RIE etching with Cl2, the PMMA was etched
away.
any one has experience in this kind of etching? which
kind of gas can etch ZnSe but not PMMA?
Thanks!!