durusmail: mems-talk: Re: SV: [mems-talk] Microform SU-8
Re: SV: [mems-talk] Microform SU-8
2006-05-30
Re: SV: [mems-talk] Microform SU-8
Gareth Jenkins
2006-05-30
They were showing it off at a conference last October. AFAIK it's still
a bit experimental so maybe this is why it's not listed on the website.
Just email Mark Shaw at Microchem for more info.


Jacques Jonsmann wrote:

> Dear Gareth,
>
> How do you manage to get hold of some dry film?
> Microchem have been playing with it for 4-5 years now, but it is still
> not listed on their web site as a product.
>


reply