Joseph Grogan wrote: > Try Piranha cleaning (sulfuric acid + hydrogen peroxide), and remember > to be careful with the solution. You may try putting the wafer on spinner then drop some SU-8 developer on the wafer and spin the wafer at very high speed usually I use 4000rpm/min.