Hi, You probably overexposed your resist. Reducing exposure time may help. bye, C. Marxer Pat Howell wrote: > Has anyone ever heard of this term. We are using it to describe a > problem we are having along an exposed region of photoresist where the > resist "pops" off leaving a semi-circle in the remaining pattern edge. > We are using a 5 minute vapor prime but we have seen the same problem at > lesser times so I dont think we are overpriming the wafers. You can > immediatly tell after exposure if mousebites are there as they leave a > bubbly area in some areas of the wafer which is visible to the eye > before develop. This problem does not occur every time (15-20%). Any > suggestions would be greatly appreciated. > > Please reply to phowell@i-o.com > > Regards, Pat Howell >