I guess that the water should be dropped on the hydrophobic area if you want to perform selfalignment by capillary force. >Thank you so much, guys. Sorry, I asked the wrong question. > > This is what I'm doing: I prepared two samples with complementary gold > patterns on top. Then self-assembly monolayers were > formed on the gold patterns to make certain regions hydrophilic and the > other regions hydrophobic. After water is dropped on the > hydrophilic regions, one sample is placed on top of the other one. We kind > of hope self alignment can happen due to the capillary force of water. But > it didn't. So we are looking for some other liquid can do this better than >