I have a problem in that I cannot get hardbaked PR (SPR-220) of my surfaces,
both gold and Si.

With the gold sitting on TiW, piranha is not really a feasible solution. I have
tried long o2 plasma ashes and overnight baths in heated prs-3000 with little
success.

Any other solutions I can try?