I don't have experience with this resist or at that thickness, but I don't think the resist should reflow at 85 C. You may try to ramp up to temp on your hard bake, or maybe a Post exposure bake. Robert -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Xiaoguang "Leo" Liu Sent: Thursday, August 31, 2006 5:25 PM To: General MEMS discussion Subject: [mems-talk] Photoresist Hard Bake question Dear all I'm using AZ926 photoressit for a thickness of 20um. However, after hardbake (85 degree C for 20minutes), the photoresist reflows and does not maintain the near vertical profile. I wonder if anybody knows anyway to prevent the reflow of photoresist during the hardbake process? Thanks a lot.