Miller Stephenson makes a product- MS-111 epoxy stripper that works pretty good to remove cured epoxies. Not sure as to what effect it might have on your sensors though, as the sample would need to be soaked in the stripper for some time. Sumant Sood Belford Research Inc. -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Mohammad Najmzadeh Sent: Monday, September 04, 2006 3:53 PM To: mems-talk@memsnet.org Subject: [mems-talk] dissolving cured epoxy glue Hello, I have attached some silicon sensors to an aluminium setup with epoxy glue and now I want to disconnect them. I am looking for a way to dissolve this cured epoxy glue. Heating of it for 3 hours on a hot plate with 200-300 degree C was one option to dissociate that glue but that was not successful.