Hi try using an oven with 140°C for 15 minutes! ---------- Initial Header ----------- > Subject : [mems-talk] Polymerisation of PDMS > Hello everybody, > > Please, someone can tell me which is the temperature and time for complete > polymerisation of PDMS ? I know there is many process on it but in your > opinion which is the best ?