---- Original message ---- >Date: Fri, 13 Oct 2006 19:31:48 -0400 >From: "Xiaoguang \"Leo\" Liu">Subject: [mems-talk] Partial Metallization of Vertical Walls >To: "General MEMS discussion" > >Dear all >I've been working on a project in fabricating cavity electromagnetic >resonators that require partial metallization of the side walls. For >example, I would like to produce a rectangular cavity in the silicon >substrate by DRIE. I would then want 2 of the 4 side walls to be >metallized with gold while keeping the other 2 silicon. I've thought >really hard about this but could not find a way to meet the >requirement. The cavity in consideration is about 1mmx1mm big. > >Does anybody have good suggestions? Thanks a lot Wow, it is a challenging task. Good thing is that 1mm x 1mm is not too hard to handle. I have few questions want to know: (1) how many cavities do you need to make? (2) What is the relative position of the two side walls? Do they have to be in the opposite side? Huaibin