durusmail: mems-talk: Nickel evaporation
Partial Metallization of Vertical Walls
2006-10-14
Partial Metallization of Vertical Walls
Nickel evaporation on PMMA!!!
2006-10-23
2006-10-23
Nickel evaporation
2006-10-25
2006-10-26
Nickel evaporation
Brent Garber
2006-10-26
Madhav,

Use a small piece of Ni wire on a tungsten helix filament if you are
doing thermal evaporation.

Brent

madhav rao wrote:

> Hello All,
>            I wanted to evaporate Nickel. In our
> university, people have used Nickel chunks, but it
> doesnt melt. Is their any other Nickel source I could
> use. Let me know about it. Also let me know from where
> I can buy Nickel Source.
>