Prakash, I've experienced this myself. SU-8 delamination during development can only be solved w/ better adhesion to the underlying layer--process params will do little to improve the situation. I purchased a Ti oxide (http://www.siliconresources.com/AP300.html) and it worked very well. Surface roughening or metal deposition will also work. Good luck. -john@MNF