Dear Richard, I suggest you contact MA/Com a Division of Amp, Inc in Lowell, Massachusetts. I believe they bond glass substrates using a gold layer. Regards, Bob. -----Original Message----- From: Richard WinfieldTo: MEMS@ISI.EDU Date: Thursday, June 11, 1998 6:50 PM Subject: Gold/Glass Eutectic >I am interested in melting a thin layer of gold into the surface layers >of a soda-lime glass substrate. I have deposited the gold layer onto the >glass but can anyone send me information on what temperature to heat the >sample to and for how long. Also should it be done in any particular >environment (nitrogen, inert etc.). > >Any information on this would be very useful. > >I would also be interested in any information on glass to glass bonding >via a gold interlayer. > >Regards, > >Richard > >................................................... > >Richard Winfield >Advanced Materials and Technologies Group >NMRC >Lee Maltings >Prospect Row >Cork >Ireland > >Tel +353 21 904377 >Fax +353 21 270271 >Email winfield@nmrc.ucc.ie >