Silicon Designs, Inc. is near Seattle. We have the capabilities to do what you ask. Are you talking about etching into the Aluminum 25 microns? It would depend on exactly what you were after whether or not we could do it. --Jason Tauscher Silicon Designs, Inc. Jason@sdi.wa.com -----Original Message----- From: Jim Intrater -- FR [mailto:jintrate@smtp.oryxtech.com] Sent: Tuesday, June 09, 1998 5:25 PM To: MEMS@ISI.EDU Subject:I need to find a company (preferably, but not necessarily, on the west coast) that can apply a resist layer to a 2.5" square of aluminum oxide and image some 1 mil (25 microns) wide, free-standing bars at at least 1 to 2 mils (25 to 50 microns) tall. Do you have any suggestions? Jim Intrater Oryx Technology Corp.