Roger,

The substrate stays at the lowest temperature during a metal deposition
when using e-beam evaporation.  Lay off the Kool-Aid.  YOU are not cool by
any means!

Brent

Original Message:
-----------------
From: Roger Shile rshile@nanoink.net
Date: Fri, 2 Mar 2007 17:40:44 -0800
To: mems-talk@memsnet.org
Subject: RE: [mems-talk] Depositing metals onto plastics and SU-8


Contrary to many postings here, E-beam evaporation is thermal evaporation;
the charge is not cool by any means.