You are right Roger. E-Beam is not going to be a cool process. In my experience Sputtering should give you near room temperature (RT + 10'C-15'C) deposition. Cheers Mantavya Sinha PhD Student Dept of ECE NUS -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Roger Shile Sent: 03 March 2007 09:41 AM To: 'General MEMS discussion' Subject: RE: [mems-talk] Depositing metals onto plastics and SU-8 Contrary to many postings here, E-beam evaporation is thermal evaporation; the charge is not cool by any means. Roger Shile