If you want to do this yourself, the tools are available to collaborators at
DOE's Pacific Northwest National Laboratory.
Glen Dunham
PNNL
509 376 4397

        ----------
        From:   Jim Intrater -- FR
        Reply To:       Jim Intrater -- FR;mems-cc@ISI.EDU
        Sent:   Tuesday June, 9 5:24 PM
        To:     MEMS@ISI.EDU
        Subject:        

        I need to find a company (preferably, but not necessarily, on the west
        coast) that can apply a resist layer to a 2.5" square of aluminum oxide
        and image some 1 mil (25 microns) wide, free-standing bars at at least 1

        to 2 mils (25 to 50 microns) tall. Do you have any suggestions?


         Jim Intrater
         Oryx Technology Corp.