2007-03-13
expose for 10s at what power?

yitianp@email.arizona.edu wrote:
>  I spin S1813 at 4000rpm 45s.
> Then hot bake 120Degree 10min
> Exposure 10s, then develop 30s.After 30s, I can't see anything.
> Why???
> All paper recommend the develop time 30s.